Site: Home > Home > News and events
With both coatings tested it performedbetter higher dry film thickness.Higher functionality UV-cured coatings faired better than lower functionality.Temperature rise due to frictional heating with the corresponding change in the coefficient of friction, has an effect on the results of the test.The RCA wear test is significantly influenced by coating thickness and substrate material’s hardness.PMMA performed better than PC and both coatings performed better at higher dry film thickness.
In the Taber wear test the higher cross-linked coating performed better and the coating thickness had a positive effect. PC at the higher dry film thickness performed better. There is a minor difference in pencil hardness with increased coating thickness in thin films. However, there was a substantial difference based upon the substrate’s material hardness itself.